Innovative Sample Holder for Large and Odd-shaped Metallographic Samples

Securing large and irregular specimens for grinding and polishing has never been easier.

View recording

录制的在线研讨会

Innovative Sample Holder for Large and Odd-shaped Metallographic Samples

Securing large and irregular specimens for grinding and polishing has never been easier.

Traditionally, large weld samples and irregular shapes must be ground by hand; a process that has poor ergonomics, poor reproducibility, and high variability among users. The Struers Flexible Sample Holder is designed to hold large and odd-shaped samples for automated grinding and polishing on the Tegramin-30. Please join us as we discuss the possible application of the Flexible Sample Holder on the Tegramin-30 for improved ergonomics and productivity in the metallographic preparation of large and irregularly shaped samples.


In this webinar, attendees will learn how to:
  • Improve health and safety with a more ergonomic process compared to manual sample preparation
  • Increase reproducibility with a more consistent process for irregularly shaped samples
  • Save time and increase productivity with high efficiency preparation surfaces vs. a series of SiC papers